hi jacob,
From what i can understand almost all the materials have P-nos assigned in that case you need to categorize the materials which are going to be used list out all the corresponding P-nos and make a WPS accordingly. You can use ASME section IX to check the P-no.

Regards

Chris

On Wednesday, April 8, 2020 at 8:20:23 AM UTC+4, charles wrote:
Hi experts,

I am currently assigned in a new piping project which uses asme sec ix and asme b31.3 . There are impact requirement also. The metals used are cs, ltcs, p22,p11, ss316,ss321,ss304 etc.

My confusion is that there are lot of combinations of piping classes which use the same material. How can i qualify wps for this piping project for all these materials.?  Any suggestions are welcome.

Regards,

Jacob.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bdf958b6-5666-4827-812f-9df0fe5dda84%40googlegroups.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...