Re: [MW:30733] Joining/welding grade X65 with X60?

Please get design/piping engineering concurrence and get it approval by the client before fitment.

On Apr 11, 2020 12:41 PM, "Rouji" <a.m.alrouji@gmail.com> wrote:
Greetings,

We have welded X60 crude oil pipeline, and we want to replace a small portion of the pipeline, can we use X65 as replacement?.
Because we have stock of X65.

Thanks.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/eadfb524-1fc1-4f05-adae-de22c88a9b74%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANiuf9e8F7Y2ecztev-uXg-k-VYTM3NeksdYrjVvr%3DBcW%2ByVFA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...