Dear Harenath,

       Due to improper storage, the thermowell of Inconel 601 got corroded. For these items can we do pickling and passivation? 

On Wed, Apr 15, 2020 at 7:28 AM harenath jha <harenathjha@gmail.com> wrote:
What is the conditions of material.
Is it heat treated normalised or something else.

On Wed, Apr 15, 2020, 10:31 Chiranjeevi A <chiranjeevipuvvula@gmail.com> wrote:
Dear all,

  Can any one suggest the specification or standard procedure s to be followed for pickling and passivation of inconel pipes and flange surfaces

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN4%2Bm0xJKPZj%2Bf35s8imSXNUXKDy%3DEKgyqDtZadtu62dHMgHmw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPRS9UOdz0Z-ti2%3DSPn1p1wh9g_1XHWJnG_TH%2B4OJbOMMg1Zkg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN4%2Bm0zGzo1KpqwbYDZ_NdHVkSfM3W2JNgb%2BSwVwnnhffkFC7w%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...