Re: [MW:30746] Run-Out Length for SMAW Process

I am not sure with the below mails but I can give explanation to Run-out Length.

In SMAW process, the distance welded by a single electrode (350/450mm length) and it is related to welding speed

Thanks & Regards

J.Gerald Jayakumar




On Monday, April 13, 2020, 07:17:45 PM GMT+7, Vishwas Keskar Welding Manager Pune India <vvkeskar123@gmail.com> wrote:


PL. EXPLAIN MORE 

What is this ?

> 100 mm is min 150 mm
< 100 mm is min 100 mm

Or you can apply simple logic:

Thickness of base metal / each layer height = No of layers * 10-20  mm (staggering length at each layer depending upon the process)



On Sunday, April 10, 2016 at 8:25:07 PM UTC+4, Maulik H. Thakkar wrote:

Dear sir,

Recommended run in run out length for base metal thickness;
> 100 mm is min 150 mm
< 100 mm is min 100 mm

Or you can apply simple logic:

Thickness of base metal / each layer height = No of layers * 10-20  mm (staggering length at each layer depending upon the process)

Regards,
Maulik

On Apr 10, 2016 2:25 PM, "Kurniatullah Sirajudin" <kurniatull...@gmail. com> wrote:
Dear Expert,

A week ago, i received comment regarding welding for smaw process.

My client ask to me, run-out length for smaw process.

I don't know what is run-out length.


Please advise me 


Thank you & Regards

Kurniatullah Sirajudin

--
http://www.linkedin.com/ groups/MaterialsWelding- 122787?home=&gid=122787&trk= anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to material...@ googlegroups.com.
To post to this group, send email to material...@ googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/ msgid/materials-welding/ bb9ef69c-8c36-42e8-b090- 7dd6d32d8af3%40googlegroups. com.
For more options, visit https://groups.google.com/d/ optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/e21dba0d-3601-4908-a012-deccee00c495%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...