Try Kobe Japan, TGX Filler wires.
Thanks & Regards
J.Gerald Jayakumar
On Saturday, April 25, 2020, 11:01:20 AM GMT+7, Saji Jos <sajijosp@gmail.com> wrote:
---------- Forwarded message ---------
From: Saji Jos <sajijosp@gmail.com>
Date: Fri, Apr 24, 2020, 3:21 PM
Subject: Fwd: SS to SS welding
To: <materials-welding@googlegroup.com>
From: Saji Jos <sajijosp@gmail.com>
Date: Fri, Apr 24, 2020, 3:21 PM
Subject: Fwd: SS to SS welding
To: <materials-welding@googlegroup.com>
Dear experts,
Please advise the suitable filler wire to weld between SS to SS without purging.structural work.
With regards.
Saji Jos Purathoor.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKZDJ1eUB_%2BqE9NENL067b_7u9Eu5_Be-1syzeSuAndOY7zJpg%40mail.gmail.com.
Comments