Wednesday, April 15, 2020

Re: [MW:30770] Pickling and passivation

Please refer packing, transportation and preservation procedure of the manufacturer.

That might contains the preservation details otherwise better to get advice from the manufacturer.

On Apr 15, 2020 10:30 AM, "Chiranjeevi A" <chiranjeevipuvvula@gmail.com> wrote:
Dear all,

  Can any one suggest the specification or standard procedure s to be followed for pickling and passivation of inconel pipes and flange surfaces

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN4%2Bm0xJKPZj%2Bf35s8imSXNUXKDy%3DEKgyqDtZadtu62dHMgHmw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANiuf9fU%3DNymc6oGHQJPmU4ZQoNX5%3D%3DJ-Oe-j7Rzxk1%3D6DLKCQ%40mail.gmail.com.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...