Re: [MW:30797] Heat input and cooling

Yes. More heat input will be cooled slowly depending on somany condition where as less heat input will be cooled faster . 

On Sun, 19 Apr 2020 10:30 am Student, <nabeel233@gmail.com> wrote:
Dear all
I am confused about the following statement. Can anyone tell me the reason.

High heat input causes slow cooling and low heat input causes fast cooling.

I understand that cooling is a function of temperature differences between the metal and ambulance system. If high heat input causes high temperature then temperature differential should be higher than low heat input.
Can any one tell me the reason.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/16692389-12f7-4b45-8ad4-e03a92e6c9b2%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOAAH4DQHECmDTee8gOOWi2Mr2_Z0LkWtASbRHWqVQiFg%40mail.gmail.com.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...