Re: [MW:30767] Pickling and passivation

ASTM A380 is a good ref.  It give a list of possible solutions to use and some basic guides. 

Regards 
Sameer 

Sent from my Huawei phone


-------- Original message --------
From: Chiranjeevi A <chiranjeevipuvvula@gmail.com>
Date: Wed, 15 Apr, 2020, 12:47 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:30766] Pickling and passivation
Dear Harenath,

       Due to improper storage, the thermowell of Inconel 601 got corroded. For these items can we do pickling and passivation? 

On Wed, Apr 15, 2020 at 7:28 AM harenath jha <harenathjha@gmail.com> wrote:
What is the conditions of material.
Is it heat treated normalised or something else.

On Wed, Apr 15, 2020, 10:31 Chiranjeevi A <chiranjeevipuvvula@gmail.com> wrote:
Dear all,

  Can any one suggest the specification or standard procedure s to be followed for pickling and passivation of inconel pipes and flange surfaces

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN4%2Bm0xJKPZj%2Bf35s8imSXNUXKDy%3DEKgyqDtZadtu62dHMgHmw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPRS9UOdz0Z-ti2%3DSPn1p1wh9g_1XHWJnG_TH%2B4OJbOMMg1Zkg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN4%2Bm0zGzo1KpqwbYDZ_NdHVkSfM3W2JNgb%2BSwVwnnhffkFC7w%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/szqe58oj0d2s-fsxwiq7empro-28y0x8349oh4-e94ibiemw9wk-b8ubefi1w4nd97l3m5hmjo7a8k8d0n-1ohidp-d6gog7cobiu5-i7059e8poasfw8qqk14c865ox9qi4-3hq4c3-of0u1a-7z7hr5.1586938838077%40email.android.com.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...