Code: ASME IX

In order to qualify a WPS, one client proposed to me to weld and qualify only one PQR test plate composed of 2 plates with 2 different thicknesses (12,5 x 9,5mm).

Does this proposal make any sense, regarding obtaining more open qualifications in terms of Base Metal thickness, I mean, 1.5 to 25mm?

My belief is that must be welded 2 test plates 9,5 x 9,5mm and 12,5 x 12,5mm. 

Is my interpretation of 2 different plates, too rigorous and narrow-minded?

Thanks in advance.

Fernando Lescovar Neto 


Livre de vírus. www.avast.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANv%2BETaVcJLSMCHUb-JNtaGQyKh3K9KZxTtOY4_tHxM9iw%2BQvg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...