Re: [MW:30737] Joining/welding grade X65 with X60?

Dear All
    Certainly you can weld the  different grade pipes use E6010 for root pass and E7010/E7018-1 for other passes.If the requirement of impact test better to use E7018-1.  
Madhusoodanan Nair.G
 Mob- 7977762694,9967901872

On Sat, Apr 11, 2020 at 12:41 PM Rouji <a.m.alrouji@gmail.com> wrote:
Greetings,

We have welded X60 crude oil pipeline, and we want to replace a small portion of the pipeline, can we use X65 as replacement?.
Because we have stock of X65.

Thanks.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/eadfb524-1fc1-4f05-adae-de22c88a9b74%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAE12Qq5KBSrhJKS6c3YMorxzLJ7tqTo4FrofqEy%3D8-H2r59Pmw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...