Re: [MW:30741] Can i weld A36 or equivalent S275JR with E7018-B2L?

What is your MDMT (minimum Design Metal temperature) at which Impact test to be conducted.

Try E 7018-C3L as it provides Impact test upto to -50degC and also contains Nickel.

E 7018-B2L is a chromium Molybdenum electrode which do not contain much Nickel

Thanks & Regards

J.Gerald Jayakumar



On Monday, April 13, 2020, 10:46:39 AM GMT+7, chris <chrissabu28@gmail.com> wrote:


our customer specifies ultra low carbon content with elevated nickel. Is there any other welding that i can use in this case?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f52cfb16-c52a-436a-a0af-7437a3aa51c8%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...