Re: [MW:29543] REG : HARDFACING(ST-6) PRECAUTIONS OVER Cn3Mn CASTINGS

Dear sir ,
               The application was oil gas valve spares.the overlay filler material make kennametal PTA powder.

On 29-Apr-2019 7:05 PM, "RAHUL Rathod" <welder.tigarc6g@gmail.com> wrote:
Dear Venkatesan 

Can you tell me what is your work Application, as per my knowledge some welding consumables have a natural tendency to crack due to high hardness if the crack is transverse, then no problem & please tell me which welding consumable you use & how much hardness its give as welded?
  

With Regards


Rahul J Rathod 
Welding Technician 

mob +91 9727076573

whats up +91 81155889118

 view my profile onLinkedIn view my profile on facebook my skype id


On Mon, 29 Apr 2019 at 12:47, <srimasstech@gmail.com> wrote:
DEAR EXPERTS 
                               WHILE HARDFACING DONE IN PTA WELDING OVER CN3MN MATERIAL WE FOUND SMALL (3-4 MM LENGTH) CRACKS IN EVERY WHERE.PLEASE GUIDE US WHAT ARE ALL THE PRECAUTIONS WE CAN MADE BEFORE WELDING ?

REGARD'S
M.VENKATESAN
SRIMASSTECH 
CHENNAI

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35754] interpration

  Interpretation #: BPV IX-18-34  Record Number: 18-771  Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...