QW-380 and QW-383 are crystal clear. The best way to go ahead is to implement QW- 383.1(b)
Στις Δευ, 20 Μαΐ 2019 στις 3:09 μ.μ., ο/η K K <karan.hbl@gmail.com> έγραψε:
--
Dear All,
We have three sort of clad,
CS + 825 clad pipe (filler metal ERNiCrMo-3)
CS + 625 weld overlay pipe (filler metal ERNiCrMo-3)
CS + 316 clad pipe (filler metal ER 309 Mo)
As per ASME IX, if welders need to be qualified in clad pipe or they can be qualified in CS regular pipes (QW-383)
Please give me your feedback.
Thanks and Regards
K K
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7b831e8e-2e13-466d-abee-53248af13818%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40Auh%2BwxGUk5DBT-cest_xYVX5ToDXX1Xdk28_wrxZVLKA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Comments