[MW:29623] Zirconium Tube Annealing & D'end Forming

Dear experts,

Need your expert advice for D'end Forming for Zirconium material (P-No.61)

Plate thickness - 18mm

What is the time and temperature suggested for D'end forming?

What is the annealing heat treatment cycle for Straight tubes for zirconium material?

Pl share of any proc.available.


Regards,

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMpWL2pGchAj7px9304koY2HsdOzLqx63f%3DTgVeMJDjB_4T%2BEQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...