If you achieve this you will get the Nobel price. You cannot weld aluminum to steel since Al anf Fe do not form solid solution. You have to use intermediate pieces of explosion bonded Al and steel

Στις Παρ, 10 Μαΐ 2019, 09:02 ο χρήστης Ram <rameshsmit@gmail.com> έγραψε:
I need to weld High Strength Low Alloy Steel to Aluminium Alloy 5052-H32 by MIG Welding Processes. What kind of MIG filler wire I should select.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/e88411a3-e3eb-408d-b975-24f7e65e072a%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40ACE0Dnn0sri%3DoomqBJ7Weeu5vK_UDD0464X5c55-J7ag%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...