Friday, May 24, 2019

Re: [MW:29636] I need to do dissimilar weld joint (6xxx series Aluminium to Steel). What filler wire should I choose?

Hi,
Please find the below link from ESAB regarding welding of Aluminum to steel. It can be possible by using Bimetallinc inserts. The file which I sent you for similar and dissimilar welding of aluminium and its different grades.



Thanks& Regards,

 

(Karthik)

Karthikeyan.S

QA/QC Manager
Agon Pacific Co.,Ltd.
M: +66-655-174-397, +66-892-512-282

E-mail : karthik6684@yahoo.com



On Friday, May 24, 2019, 1:26:14 PM GMT+7, 'Karthik' via Materials & Welding <materials-welding@googlegroups.com> wrote:


Hi,
The attached file might be useful to you.

Thanks& Regards,

 

(Karthik)

Karthikeyan.S

QA/QC Manager
Agon Pacific Co.,Ltd.
M: +66-655-174-397, +66-892-512-282

E-mail : karthik6684@yahoo.com



On Thursday, May 23, 2019, 6:44:48 PM GMT+7, Ram <rameshsmit@gmail.com> wrote:


I need to do dissimilar weld joint (6xxx series Aluminium to Steel). What filler wire should I choose?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7206cf51-d3f4-413a-838e-3036e9ad1a26%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1605684784.4306536.1558663626710%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...