[MW:29636] Suitable filler and and electrodes

Dear experts,

I have to qualify the the PQR as per (ASME Sec IX 2017)  for the the following

Material: (SA516Gr.60+SB127)+(SA516Gr.60+SB127), that is SA265 Clad plate.

Process: GTAW+SMAW (Image attached below)

Groove: single "V" groove weld.

Thk.:22mm+3mm of clad.

Kindly advise the suitable filler wire and electrode.SFA no. & Classification no. 


Regards.
Dhakshnamoorthy.J

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHHcqJcqY-zQf8FGmv4diMbYjs75YvKRnC_-U8_sxTHXX2KChg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...