Monday, May 27, 2019

Re: [MW:29643] Impact test at -210 Deg C

Sir

For which material reqd. Impact at - 210.
I think every body have facilities upto - 196 only. 
Re check your requirements and procede. 

Regards 
A p gupta 
ThyssenKrupp 
QC manager 
Baroda 

On Mon, 27 May 2019 at 15:09, chiluka venkatramulu
<ramuluchiluka@gmail.com> wrote:
Dear Mr.Guptha,
Thank you for your information. But I enquired with them, they are conducting impact up to -196 Deg C only. Pl let me know if any other labs are there.

Thanks & Regards,m
Venkatramulu C

On Sat, May 25, 2019 at 2:18 PM anand gupta <gupta_0576@yahoo.co.in> wrote:
Check met heat engg. 
Vadodara Gujarat  india. 

They have facilities to do impact at - 210 deg c. 

Regards 
A p gupta 


On Sat, 25 May 2019 at 11:14, chiluka venkatramulu
Dear All,
Anybody know the mechanical labs, who can conduct impact at -210 Deg C in India.

Thanks & Regards,
Venkatramlu.C

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF98%2BdGH4d4JqvdjFKb6sPFfo2bp4NFpA09MBYG3%3DUngPZb4qg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/720400546.5889384.1558958254260%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...