Monday, May 20, 2019

[MW:29607] Re: WPS

You may select for SMAW

ASME SFA 5.4, Classification E2209—duplex filler material.
ASME SFA 5.4, Classification E309L—high-alloy austenitic filler material
ASME SFA 5.4, Classification E309LMo—high-alloy austenitic filler material

Read more in API RP 582 2016 Table A.3

Bien ND



On Sunday, May 19, 2019 at 12:34:24 PM UTC+7, merghni wrote:

Dear Colleague;


I have a question ,please i want to know how to select the filler metal to weld dissimilar metal ,because i have WPS , the information :  P1 to P10H ,Grade API 5L,PSL 2  , X65Q to Grade ASME A790 S31803 and  i found the electrode ER2209 for root and E2209-16 for fill is this selection acceptable or not i need advice  .
I review ASME IX but i didn't find any information about this.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c69e16b2-7948-4eff-b322-d493d636c606%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...