Re: [MW:29657] ERNiCU7 TIG hot wire cladding weldabilty

For overlaying steel, first, apply a barrier layer of nickel-base overlay shall be used first (high Ni%).

Regards
Ramin  Kondori
Sr. QA/QC & Welding Engineer
-----------------------------------------------------------
PG-Dip. in Welding Engineering (IWE  AT  0070)
BSc. in Civil Engineering (IUT)
BGAS Painting Inspector
ASNT Level I&II
                        
IIW-Logo-Colour-small


On Thu, May 30, 2019 at 5:45 PM 'Neilash Kumar' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Gents , 
Currently am developing procedure using hot wire TIG process using ERNICU7 CLADDING , 
Thickness of cladding minimum 3.2mm , 2layer only
Fe value to be less than 2.5 after 2 layer .
Can you please share your experience regarding the weldability issue and precaution to take care during weld procedure?
Regards 
Neilashkumar 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1722606054.6338032.1559152590346%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEagfUiNSdgNp9Pe_XzeB7C_%3DY64ATGcU4U2ZikYuWTmoRxr9g%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...