Dear experts,
-- Please let me know welder qualification range.
Details as below :
Actual Values
Pipe- Groove
1) P 43 To P 43 (SB-444)
2) GTAW ( Manual )
3) Thickness -5.54mm
4) SFA-5.14
5) F No- 43
6) Filler metal -ERNiCrMo-3
7) Position -6G
If I am not Wrong please check below i have mentioned Range Qualified.
Groove and Fillet Weld
1) P No - 1 thru 15F,34,41 thru 49
2) GTAW ( Manual )
3) SFA No- 5.xx
4) Thickness - 11.08mm
5) F no- 34,41,46
6) Filler metal - Any
7) Position - All
Please give me your feed back.
Regards
Kiran
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a0641006-7a9d-438d-8a30-75a59731576f%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Comments