Re: [MW:29582] Welding HSLA to Aluminium

Not possible by Arc welding..
Try other alternatives..


PREM S NAUTIYAL
CELL : 9769316004





From: Ram <rameshsmit@gmail.com>
Sent: Fri, 10 May 2019 11:32:55 GMT+0530
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:29578] Welding HSLA to Aluminium

I need to weld High Strength Low Alloy Steel to Aluminium Alloy 5052-H32 by MIG Welding Processes. What kind of MIG filler wire I should select.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https:roups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/e88411a3-e3eb-408d-b975-24f7e65e072a@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1557468175.S.7557.20340.f4-234-164.1557504367.7207%40webmail.rediffmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...