Dear Group
Just to share with you this indication.
It´s about a failure in the bottom zone of pressure vessel separator.
This is a thickness lost due to corrosion by bacteria or MIC as is mentioned in API 571
This indication has more than 2 meter in longitude and 0.6 meter in wide.
Nominal wall thickness 3/8".
Failure presented after 15 years in service of pressure vessel.
Regards
Miroslav Tadic
Integrity Engineer
API 581 IPC # 60883
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/B1C5C970BEA29243935FA5EB72F113C80362EFAB0D%40BOLEXVSG11.chaco.com.bo.
For more options, visit https://groups.google.com/d/optout.
Just to share with you this indication.
It´s about a failure in the bottom zone of pressure vessel separator.
This is a thickness lost due to corrosion by bacteria or MIC as is mentioned in API 571
This indication has more than 2 meter in longitude and 0.6 meter in wide.
Nominal wall thickness 3/8".
Failure presented after 15 years in service of pressure vessel.
Regards
Miroslav Tadic
Integrity Engineer
API 581 IPC # 60883
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/B1C5C970BEA29243935FA5EB72F113C80362EFAB0D%40BOLEXVSG11.chaco.com.bo.
For more options, visit https://groups.google.com/d/optout.

Comments