Monday, May 13, 2019

[MW:29583] Thickness Qualification Range as per AWS D 1.1

As per AWS  D 1.1. if I do WPS qualification on 90 mm thickness Plate with Impact at -40 deg then how much we qualified for thickness range ?
Please advise me .
Thank you in advance.

Regards,
Rajendra Jadhav

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKtLVJxXpx%2BZ7N7uGzEbYmK_O5vm41kn0m_QomkMA958aYCbhg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...