Re: [MW:29571] Electrode for Material SA516 Gr70

E 7018 my suggestion...


Regards
Afzal...

On Wed, May 8, 2019, 4:38 PM George Dilintas <dilintas@gmail.com> wrote:
I would suggest E7018

Στις Τρί, 7 Μαΐ 2019 στις 3:09 μ.μ., ο/η Kiran <karan.hbl@gmail.com> έγραψε:
Dear All,

Please refer below mentioned details and please let me know, can I use this details in PWPS as per D1.1.
 
1) Material -SA 516 Gr.70 to SA 516 Gr.70

2) P No- 1 Group No - 2 to P No- 1 Group No - 2

3) F No- 4
 
4) A No-1

5) SFA No- 5.1

6) AWS No(Class) -E-6013.

I have debut about electrode.  

If any thing please wright briefly.


Thanks and Regards

Kiran 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a45e40b7-5849-44b8-80b2-9c2551ce957c%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40D9VGKD3ZhKnkB15mXi%2BUiGEpCBzRWR4eGKOkqbwXHpxA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPjThrOij2TssfBt%3DdbJX_xGvdFCnJdNeLY2fgCMJ3xo_ffcOw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...