Re: [MW:29430] Re: Multipass - Heat Input

I would advise to read QW-409.1 and the appendix H in ASME IX.
When impact test is applicable, heat input becomes a supplementary essential variable.
New PQR is required when heat input is increased.
So, considering the calculations of heat input given in QW 409.1 you have to record the max heat input per pass

Στις Κυρ, 31 Μαρ 2019 στις 5:34 π.μ., ο/η Gowtham Rajendran <rajgowthamiwe@gmail.com> έγραψε:
I.e Heat Input is different in various layers for the fillup passes.

On Sat, 30 Mar 2019 at 18:01, Gowtham Rajendran <rajgowthamiwe@gmail.com> wrote:
Hi ,
       A very good evening to you all.
       My doubt is in establishing the heat input for multipass welding , (root , fill & cap) , for the fillup passes my parameters are different for different layers , which one should i consider for establishing the Heat Input because in this CVN Requirement apply & the heat input cannot be increased as per the code (Be it ASME Sec IX or AWS D1.1).
       How to solve this problem? Kindly help.

Regards,
Gowtham.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...