Sunday, March 24, 2019

Re: [MW:29364] Qualification of 2 welders in one Test Piece (Pipe 12" inch)

See attached


Thanks and regards
Hisham Almetwally
QA/QC Mechanical Engineer & Welding Engineer
Mob: +971564337326 & +971526679935

On Sat, 23 Mar 2019, 4:23 pm 'Ibrahim Ramadan Hassan' via Materials & Welding <materials-welding@googlegroups.com wrote:
Boxbe This message is eligible for Automatic Cleanup! (materials-welding@googlegroups.com) Add cleanup rule | More info
Dear Sir
I am inquire about the Welders qualification test as Per ASME IX - QW-302 & QW-304
If I make WQT for qualification of (2) welders welding together in one test Pipe 12 " inch
hence the total circumference of Pipe 12 " inch = 957 mm so, Each welder will weld more than 150 mm as required by ASME IX And all the Pipe Circumference welded by each welder will be radio graphed.
Is that Acceptable is or not to qualify 2 welders in one test piece (Pipe 12" inch)?

Kindly reply on my inquiry.

Best Regards
Eng. / Ibrahim Ramadan Hassan
Section Head Mechanical QA/QC
PETROJET - Jordan Branch
Egypt Mob. : 00201000948366
Jordan Mob. : 00962791023621




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...