Hi John,
Please make sure you have enough coupons and you conduct all the tests as per both the codes. Upon satisfactory results, you can write WPSs seperately for each code.
Thanks and Best Regards,
K.Rajagopal

On Wed, Feb 6, 2019 at 5:03 PM HerculanJohn <hjpr820@gmail.com> wrote:
Dear Sirs,

Can you please throw some light on WPS meeting both EN Standard & ASME Sec.IX.

Is there any additional test done on test coupon or coupon material needed i.e, impact testing. 

Or WPS is made meeting project requirements only.

Kindly advise.

Best Regards,
John,
08806621979.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...