Re: [MW:29430] How to make WPS and PQR for A106 Gr. B for my study

if no impact test requirement, the thickness range would be 1,5 mm to 2X5,9=11,8 mm

Στις Παρ, 29 Μαρ 2019 στις 5:35 π.μ., ο/η Emil Multazam <emil.multazam@gmail.com> έγραψε:
Dear Experts..

Could anybody help me, how to determine range thickness pipe A106 Gr.B for WPS ?
I have test coupon with thickness 5.9mm

Regards,

Emil Multazam
Manufacturing Engineering
College at University of Surabaya

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...