[MW:29355] Re: Weld Repair of ZG35CrMo (34CrMo4)

Dear experts,

Thanks for your reply,
The roller is in service and we do not have WPS/PQR.
During evaluation it is observed that crack dept is around 25-40mm. 
Total roller thickness is 280mm. 

Sent from my iPhone

On Mar 20, 2019, at 17:23, nithindsilva4u@gmail.com wrote:

Dear Experts,

We have observed a crack on a roller of material ZG35CrMo (34CrMo4). We want to do weld repair. Could you please advise the below;
1. Consumable to be used
2. Preheat temperature 
3. Inter pass temperature 
4. Any post heating
5. Final heat treatment temperature 
6. Any special precautions?

Sent from my iPhone