Thursday, March 28, 2019

RE: [MW:29411] PMI Testing -ss316

ASME II A, B,C  has a table for each material and show tolerance  CR 18-20, NI 11-14  ETC shall be in that range.


Carlos Arturo Oliveros Diaz  +573023482020

            ws+584245923932



De: materials-welding@googlegroups.com <materials-welding@googlegroups.com> en nombre de Harish Kannepalli <harishkannepalli@gmail.com>
Enviado: jueves, 28 de marzo de 2019 7:08 a.m.
Para: materials-welding@googlegroups.com
Asunto: Re: [MW:29410] PMI Testing -ss316
 
Hi,
    PMI technique is by xrf, which is semi quantitative in nature. The standards refer to test methods which are accurate than PMI, hence those tolerances cannot be applied for PMI.

On Thu, 28 Mar 2019, 15:44 Sameer, <sameer.landgebv@gmail.com> wrote:
Dear Experts ,
During PMI testing of SS316 material Ni observed - 9.86% , required range is 10-14%.
observed value will be accepted or not . Please provide your valuable comments .

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...