Wrong,

you should read UCS-79 carefully. The HT is a function of P-No and extreme fiber elongation, and service conditions.
UCS is applicable for carbon steel materials
For high alloy (example stainless steel) pls refer to UHA-44
For enhanced ferritic steels pls read UHT-79.

Friendly advise: read the Code carefully

Στις Κυρ, 31 Μαρ 2019 στις 5:34 π.μ., ο/η Brijesh Maurya <brijeshmaurya492@gmail.com> έγραψε:
thickness above 16 mm as per UCS-79 of ASME sev.VIII div.1

On Thu, Mar 28, 2019 at 4:53 PM vikram saipogu <saipoguvikram@gmail.com> wrote:
Dear All,

Under which Condition,

Heat Treatment is mandatory for dish end ?

Thanking you.

Best Regards,

Vikram Saipogu


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...