Thursday, March 28, 2019

Re: [MW:29407] PMI Testing -ss316

Hello,

If you checking on the weld, it should be the A number mentioned in WPS.
If you checking on the base material it should be respective base material values (Example A182 316, A312 316 Etc). Refer SEC II A.

Thanks with warm regards,

Pramodh M.R
Sr.Inspector (Welding/Coating)


On Thursday, March 28, 2019, 1:21:47 PM GMT+3, Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:


what is the tolerance for PMI values

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Thu, Mar 28, 2019 at 3:44 PM Sameer <sameer.landgebv@gmail.com> wrote:
Dear Experts ,
During PMI testing of SS316 material Ni observed - 9.86% , required range is 10-14%.
observed value will be accepted or not . Please provide your valuable comments .

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...