[MW:29399] Re: Electrode selection for 3G40 to ST52-3

I believe 3G40 is ductile cast grade according to the DIN specification. 
In this case you can go Magna 770 welding consumable.

Thanks &  regards
Sandeep Kumar

On Tuesday, March 12, 2019 at 6:17:03 PM UTC+3, saeed sarir wrote:

hello dear expert
? Do you know what kind of electrode is suitable for welding 3G40 to ST52-3

Thanks

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...