Re: [MW:29388] SA 333 Gr 6 Heat Treatment

Dear Sir,

Agreed with Your Screenshot

Can you please let me know weather there is any Exception for HOT Finish Pipes ?

TC Of without Heat Treatment for HOT Finish Seamless Pipe ( SA 333 Gr 6 ) is acceptable or not ?

Best Regards,
Vikram Saipogu



On Tue, Mar 26, 2019, 9:32 AM Xhoaib <shoaibdanvi91@gmail.com> wrote:


On Tue, Mar 26, 2019 at 8:52 AM vikram saipogu <saipoguvikram@gmail.com> wrote:
Dear All,

Do SA 333 Gr 6 Pipe need Heat Treatment ?

*For Hot Finish Seamless Pipes

Best Regards,
Vikram Saipogu

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...