Re: [MW:29392] Qualification of 2 welders in one Test Piece (Pipe 12" inch)

you can qualify four nos of welder also

On Tue, Mar 26, 2019 at 4:09 PM 'Ibrahim Ramadan Hassan' via Materials & Welding <materials-welding@googlegroups.com> wrote:
If the Position of the WQT is 6 G , that one Test coupon (12 " inch ) - Can qualify Two welders or Not ? hence the total length welded by the two welders in parallel
 will be radio graphed.

Best Regards
Eng. / Ibrahim Ramadan Hassan
Section Head Mechanical QA/QC
PETROJET - Jordan Branch
Egypt Mob. : 00201000948366
Jordan Mob. : 00962791023621






On Tuesday, March 26, 2019, 9:37:50 AM GMT+2, chandraknat vaidya <vaidyac10@gmail.com> wrote:


Yes. Provided All other essential variables should same.
CLV

On Tue, Mar 26, 2019 at 7:59 AM George Dilintas <dilintas@gmail.com> wrote:
It depends also on the positions you want to qualify. Pls read the Code carefully, to check if they have to weld an entire circumference

Στις Σάβ, 23 Μαρ 2019 στις 2:07 μ.μ., ο/η 'Ibrahim Ramadan Hassan' via Materials & Welding <materials-welding@googlegroups.com> έγραψε:
Dear Sir
I am inquire about the Welders qualification test as Per ASME IX - QW-302 & QW-304
If I make WQT for qualification of (2) welders welding together in one test Pipe 12 " inch
hence the total circumference of Pipe 12 " inch = 957 mm so, Each welder will weld more than 150 mm as required by ASME IX And all the Pipe Circumference welded by each welder will be radio graphed.
Is that Acceptable is or not to qualify 2 welders in one test piece (Pipe 12" inch)?

Kindly reply on my inquiry.

Best Regards
Eng. / Ibrahim Ramadan Hassan
Section Head Mechanical QA/QC
PETROJET - Jordan Branch
Egypt Mob. : 00201000948366
Jordan Mob. : 00962791023621




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...