Saturday, March 23, 2019

Re: [MW:29358] WELDING DEFECT AT ROOT

Dear Muhammed Ibrahim:

RT must have shown this one way or another otherwise your RT system might not be effective enough.
At least some indication of a Root Concavity or so must be evident in your RT film.

My recommendation is that do not focus on rejecting or accepting this particular weld but rather raise this issue as a QA finding and try to find out why your RT examination system has not been able to detect this potential defect. If your RT system has not detected this one, you'd better take it seriously. 

Regards
Ramin  Kondori
Sr. QA/QC & Welding Engineer
-----------------------------------------------------------
PG-Dip. in Welding Engineering (IWE  AT  0070)
BSc. in Civil Engineering (IUT)
BGAS Painting Inspector
ASNT Level I&II
                        
IIW-Logo-Colour-small


On Fri, Mar 22, 2019 at 2:58 AM Muhammed Ibrahim PK <ibratech@gmail.com> wrote:
Gents, 

I am getting the attached image in boroscope inspection at root. But RT not showing any density variation or undercut. Please give your comment on it. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...