You can check EN 1011 - 2 for preheat requirement as well.
On Fri, Mar 29, 2019, 7:34 AM Souravbohray <ermechsouravbohray@gmail.com> wrote:
i want to know were is given asme sec 9 what will be interpass temprature.is there any value given in code for interpass temp it is given only + 55 c but what temperature we can go +55 c preheating temp given in asme sec 8--
On Tuesday, 14 September 2010 18:13:18 UTC+5:30, limesh M wrote:Dear All,
Design Code: ASME B31.3 Welding Code: ASME SEC IX
I have a Low temperature carbon steel impact tested PQR with a PWHT range of 600⁰±10⁰C.Is this condition giving an exemption for me on QW406.3 to prepare a WPS with maximum interpass temperature of 200⁰C.
Maximum interpass temperature observed during specimen welding: 140⁰C
Regards,Limesh
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Comments