Thursday, October 4, 2018

Re: [MW:28391] Re: how to find exact travel speed of welder

Its a recorder which can be connected to the welding machine. When welder strikes the arc, it will start monitoring the current used, voltage, travel speed and heat input.
You can watch the demonstration in youtube, TVC Product I have used and they are good. It is called weld arc logger or weld arc monitor. see attachment 

On Wed, Oct 3, 2018 at 5:36 PM Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
Nitin could pl elaborate

On Wed, 3 Oct 2018 6:14 pm Nithin Joseph, <nithindsilva4u@gmail.com> wrote:
You can use weld arc monitor to measure the exact travel speed with heat input during welding.

On Wed, Oct 3, 2018 at 10:15 AM Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
Manual & Semiauto welder"s travel speed vary from welder to welder. 

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ASNT-Level II in PT,MT,RT & UT.
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Wed, Oct 3, 2018 at 10:56 AM sandeep kumar <sandeepdhiman63@gmail.com> wrote:
Two possible way based on my experience:

1. mark the length at the start point, keep a eye on the stopwatch, when it tickle 60, mark the location while welder is still engaged in welding, so you will have straightaway TS/ min.Most suitable in SAW, GMAW, PAW (make sure to shield eyes while mark the weld at 60 second).

2. Secondly, mark the start point, keep eye on the clock, take the last point where the welder stop, This length, divide by time taken in seconds & multiply with 60 will give TS/ min. 

The first case will not work in certain situations, e.g. 
a. while welding short runs which get completed less than a minute.
b. SMAW process with shorter electrodes & higher current as they certainly will get consumed less than a minute.
c. Intermittent fillet welds 
4. Tack weld of longer lengths etc

Both of above approaches assume there is no stop during welding during count time. The automated welding process e.g. robotic welding, laser welding, FSW are gives TS values as its a program feature as you preset these values.

Thanks & regards
Sandeep Kumar
On Sunday, September 30, 2018 at 1:22:20 PM UTC+3, ali wrote:
What is the proper way to calculate a welder's travel speed?

please answer this question according to your experience.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
Regards,
Nithin Joseph Dsilva
+971 557645785

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
Regards,
Nithin Joseph Dsilva
+971 557645785

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35346] Cast-iron welding

Any advice for cast iron welding Sent from Yahoo Mail for iPhone