Thursday, October 4, 2018

Re: [MW:28385] PQR Qualification _welding electrode

Dear Mr. Rajesh,
Please share service, Construcation and qualification code.

Regards,
Muhammad Babur Khan

Sent from my iPhone

On 3 Oct 2018, at 6:08 PM, RAJESH KUMAR <rajeshkumarbhaskara@gmail.com> wrote:

Dear Team,

For our PQR qualification ( Done in 2018) to flux coared wire for carbon steel,we use the wire clasified SFA/AWS A5.20  E71T-1C/1M/9C9M.

Today we received from our supplier wire classified SFA A5.36 E 71 T-1C 1A2-CS1.

The classification is different,so we have to issue new PQR qualification required?



Thanks & Regards

Rajesh kumar
055-5251449
Sharjah

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.