Re: [MW:28371] evaluating of micro structure

Dear Meisam.
I have forgotten to say that ASTM have some adjuncts such as '' Photographs for Rating Macroetched Steel(ADJE038101 (Plate I), ADJE038102 (Plate II), and ADJE038103 (Plate III).'' and similar like that to help us for interpretation.

Regards.

On Tue, Oct 2, 2018 at 9:52 AM meisam shokri arfaei <meisamshokri@gmail.com> wrote:
Dear Ali,
If you look for differences between primary and tempered martensite, it needs some deep knowledge and experience which some metallogheraphers have it. Also it needs a brief history of the sample, special sample preparation, special and precise etching and ... .
For more information about visual differences in microstructures you could go through ASM Metals handbook Vol. 9 - Metallography.

Regards

On Tue, Oct 2, 2018 at 8:23 AM slick ronz <vinopvarghese@gmail.com> wrote:
Dear Ali,

Can you be more specific about the Material grade you are looking for? If we consider a case of P4 material like WP11, the heat treatment required is Normalised and Tempered condition. Hence the MTC shall mention this requirement and no further evaluation is required for micro structure examination.

Hope it answered your question.

Thanks and Regards,
Vino Varghese
Qatar


On Sun, Sep 30, 2018, 09:14 Ali Asghari <asgharialigl@gmail.com> wrote:
Dear All.

Does anybody know how it is possible to evaluate the bainite or martensite of the base metal is tempered or not?
I want to know the method , frequency of testing, acceptance( such as figures) and any other issues that can say with confidently we have tempered micro structure or not?
as you know this is more crucial in sour service and is a requirement in our specification but doesn't mention detail of it.

Regards.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
M. Shokri Arfaei
ASNT NDT Level III
International Welding Engineer

Mob.:+98 912 1394023




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/8NmUN68k8eo/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...