[MW:28384] Re: PQR Qualification _welding electrode

Thanks for sharing this interesting issue.

as per my understanding you dont need to qualify new PQR if both meet the CVN requirements. As we see we are inline with same F no, same A no. although different filler wire specification with change is supplementary designation.

As per QW 404.12 and 404.33, you can just issue a new WPS based on the PQR with new designation.

Hope it will help.

Thanks & regards
Sandeep Kumar

On Thursday, October 4, 2018 at 5:14:43 AM UTC+3, RAJESH KUMAR wrote:
Dear Team,

For our PQR qualification ( Done in 2018) to flux coared wire for carbon steel,we use the wire clasified SFA/AWS A5.20  E71T-1C/1M/9C9M.

Today we received from our supplier wire classified SFA A5.36 E 71 T-1C 1A2-CS1.

The classification is different,so we have to issue new PQR qualification required?



Thanks & Regards

Rajesh kumar
055-5251449
Sharjah

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...