Re: [MW:25839] E8018-B3L can be replaced with E9018-B3L

Hello Raju,

What are your service conditions (temperature, corrosion etc.) and what are the material (or weld) requirements as per your specification?


Ramin  Kondori
Sr. QA/QC & Welding Engineer
-----------------------------------------------------------
PG-Dip. in Welding Engineering (IWE  AT  0070)
BSc. in Civil Engineering (IUT)
BGAS Painting Inspector
ASNT Level I&II
                        

On Fri, Dec 23, 2016 at 4:34 PM, GUJULA JAYARAMAN Raju <rajudhanush@gmail.com> wrote:
Can anyone suggest the electrode EQUIVALENT FOR E8018-B3L  for welding SA 387 GR 22 CL2 PLATE SEAM BUTT WELDS WITH IMAPCT REQUIREMENT  55 JOULES AT -30deg.C.

Since, in the market, only E9018-B3L is available.

​Can we use E9018-B3L instead of  E8018-B3L

Thanks & Regards

​G.J.RAJU
QC Chennai
Mob; +91 9940429224​

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO_Rx-L7DeU9mnDj2id00A0t%2B-GLEvjC66V%3DK6Fnut7a_EmG9Q%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEagfUiH5b_U0hj%2B%3DrUO_YXEq%2BCYJ8d%2B2AmT%3D-_vwWKTYq7BhA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...