ER316L have Mo greater than ER308L which increase pitting corrosion resistance , contain also NI greater than ER308l which increase toughness.

In ASME IX change of welding electrode is essential variable but ER308L and ER316L have the same "F" number so you can make another WPS on the same PQR of ER308L.

To cover your issue and take your client approved before, if he refused respect your "WPS" and C/O wrong welded joint.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/65af86f8-fa2a-48a5-aa72-bf757ee965f6%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...