Wednesday, December 14, 2016

Re: [MW:25820] Using ER316L instead of ER308L to weld 304L to 304L


The WPS is made with ASME IX ?, I think one of the main data that should be placed in your question is the building code, so that the experts who see this email can help you, if you give incomplete information it is more difficult to help you .

2016-12-14 5:02 GMT-06:00 44897 <malgireddy.2007@gmail.com>:
Dear experts,

we have situation is here one of our welder selected wrong filler material,

To weld 304L to 304L as per wps it was selected ER308L.

One of our welder welded with ER316L we have found this after completion of weld in the PMI results where MO content is showing 2.0%.

Is that acceptable to weld higher grade electrode for 304L piping. 

Regards
Reddy.M

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3b99f624-8c97-4143-8a84-82ff9352252c%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--

Ing. José Juan Jiménez Alejandro

Cel. 812 103 1155

Skype: jjjimeneza

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO5ZurJt%2B-kS-Z4QiZzsRf57WVJGX9wjSVF0%2B6Q%3D4dcT6mRSwg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...