Dear Vadival,
You have to comply with the requirements of the design code, which in this case is ASME VIII Div 1. That determines the application requirements, not the material specification.
Alan Denney
AKD Materials Consulting Ltd
-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Vadivel Mahadevan
Sent: 30 December 2016 03:40
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:25854] PWHT reqmt for welds as per API 6D
Dear Experts,
I have a Groove weld joint of thickness 40mm. The standard i need to follow is API 6D..
Welding procedures qualified under ASME sec.IX without PWHT with a test coupon of 50mm thickness of material ASTM A516 gr.70..
API 6D states " PWHT shall be performed in accordance with the applicable material specification or design code"
My material specification is ASTM A516 gr. 70 and Design code is ASME Sec.VIII Div. 1
A516 standard doesnt states welding or PWHT requirement, whereas ASME sec.VIII states - thickness above 38mm PWHT is mandatory..
Can i take the material specification to justify for not performing PWHT..
Please advise
With regards and thanks
Vadivel M
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d3a93cea-c615-43c9-9089-177d9cbcc77e%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
This email has been scanned by BullGuard antivirus protection.
For more info visit www.bullguard.com
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/000801d2627c%240dde39a0%24299aace0%24%40denney1.freeserve.co.uk.
For more options, visit https://groups.google.com/d/optout.
Subscribe to:
Post Comments (Atom)
[MW:35692]
Dear all Can I do MPI above painting surface for cs tank Regards, Sriram Srinivasan -- https://materials-welding.blog...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment