According to the bibliography min hardness on P91 should be 191 HV
Sent from my BlackBerry 10 smartphone.
| From: Kannayeram Gnanapandithan Sent: Τετάρτη, 31 Αυγούστου 2016 - 08:38 To: materials-welding Reply To: materials-welding@googlegroups.com Subject: Re: [MW:25334] Hardness Value For the P-91 and SS material. |
Hardness only on HAZ of P91 is to be around 230Hv
THANKS & BEST REGARDS,
KG.PANDITHAN, IWE, AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349
On Tue, Aug 30, 2016 at 9:59 AM, pradip kumar Sil <pradipsil@gmail.com> wrote:
Dear Everybody,--How much is Lower & Upper hardness limit with code reference for the weldment of ASTM-A-335 Gr. P-91 To A312 TP 316 with filler combination ER-Ni Cr3.Regards,Pradip
http://www.linkedin.com/groups/MaterialsWelding- 122787?home=&gid=122787&trk= anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com .
To post to this group, send email to materials-welding@googlegroups.com .
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB% .3DAs8n-WNLDxx1b6%3Daqu_my_ rTKo8HKme9cWQsamH5NKVJMbQ% 40mail.gmail.com
For more options, visit https://groups.google.com/d/optout .
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNaPwK%3DOZMxuh0ZPWExJGYeu7qY%3D7thZ6JkX7X2oCVNiQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Comments