Thursday, June 30, 2016

Re: [MW:25032] impact results - UHT material welding

yes in Q&T steel,. before taking up for PWHT, better consult manufacturers for temperature and Time

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Thu, Jun 30, 2016 at 12:30 AM, Fernando L Neto <fernando.lescovar@gmail.com> wrote:
Dear colleagues, 

I hope this email finds all you well

Project: ASME VIII- Pressure vessel - material ASME SA517 Gr B. Thickness 9,5 mm.

 I have to qualify a WPS for welding ASME SA517 - B with impact requirements at -40 C, 

Also is required PWHT, and my first results of impact test @-40C of test plate were very low. (lateral expansion less than 0,2mm and energy less than 20J)

The declared Values of certificate of consumable is 75J @ -73C  !!!

Can the presence of PWHT changes so much the values of impact test? (certificate´s value is "as welded" and my results is "after PWHT".

Any help will be very useful. 

Thanks a lot, 

Fernando Lescovar Neto (IWE)




--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANv%2BETZM4c_%3Dh%2BeKOosPusHUqGE_5b0DZ3aO12GyNDPph3dUbw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eN35H_KrRLWqyoo%3DRgJHdN22ytW133ZrCcR%3D0fr%3DkO0yw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS