Wednesday, June 29, 2016

Re: [MW:25024] Chemical Composition

what was origina chemistry hardness  is very low

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Wed, Jun 29, 2016 at 1:37 AM, 'Mac Palola' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Dear Sirs,

Project: Coal fired power plant ASME B31.1 CODE

We received a pipe material 1 inch dia with a material of A335 P91.
This material had been welded.
During operational, 2 years after, one pipe burst out.
We send for testing to check the chemical composition. Please see attached docs.

I checked on ASME Section II Part A and it was very far from the chemical requirements of A335 P91.

My query is that, what kind of pipe material base on the result of test report.

Your reply to this query will be highly appreciated.


Regards,

Mac




--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5c7fba20-d6e9-4fc8-b7b5-472c4cf79057%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePOD7b8%2Buk3dj0LMXa5PmiDCDK6QbqCN_2opq5AJU%3DcNg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...