Wednesday, June 29, 2016

Re: [MW:25020] Relation between diffusible hydrogen and welding current

Dear George,

Thank you very much for the document shared. It's very useful.

Pravin Poornachandran


Sent from my iPhone

On 27 Jun 2016, at 20:58, George Dilintas <dilintas@gmail.com> wrote:


2016-06-27 13:30 GMT+03:00 Pravin G <htcispravin@gmail.com>:
Dear expert,

What is the correlation between diffusible hydrogen and welding current.

How does Welding current affects diffusible hydrogen ? Based on any specific code or theory?

Kindly help to explain.

Pravin Poornachandran
Singapore
Sent from my iPhone

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5DFF92D3-8F9F-4BA9-A964-E41BEB02E7CA%40gmail.com.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40D%3DamijFiN47dKq1R4LD63AL7%3DuHc38TSa%3D3bMBGe%2ByNQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...